Billet Cracking Of Zircon Brick

The basic reason for billet cracking during drying process of zircon brick is as below,
 
1. There is no full understanding of the characteristics of the three stages which are equilibrium temperature, low temperature and high temperature during the drying process, and the requirements of drying technology.
 
2. Hot air supply is short and Body can not be fully dry
 
3. The drying temperature curve is not reasonable which could not meet the requirements of the temperature curve of the billet during the drying process.
 
4. Wet control is not good, and the temperature of each section is not reasonable in the drying kiln which is failed to meet the requirements of the temperature of the body drying temperature.
 
5. Hot air and wet air is not uniform which cause temperature difference in dry kiln and thermal shocks in some place, so the thermal stress caused by this way can cause the body to break and cause the billet crack.

zircon brick


 
 
Zhengzhou Sunrise Refractory Co., Ltd can provide magnesia brick which has passed the ISO international certified, such as fused cast series brick, zircon brick, magnesia brick and so on. Over 30 years producing and marketing experience, with reliable quality, competitive price and prompt delivery, Sunrise has established long-term business and cooperation relationship with many customers in different countries and regions. For any further information, Contact us, we will do our best to help you.